Vol. 23 #1, May 1996

Die plate out or carbon build up can cause die lines and contamination of sheet products.

During the last several years, several die manufactures are offering low surface energy die treatments which mimics the effect of flouropolymer additives for polyethylene, as well as improves die cleanliness.